Leveling flux is a mixture of more pure quality zinc chloride solution and ammonium Chloride with some special additives which make this flux more expensive than others.
It is in liquid form with ideal mixing ratio.
This can be used to increase the Baume (Be) or Specific Gravity of the Flux Bath in between the Galvanizing process which increases the life of Galvanizing Pre Flux.
Some special Features
- It is in liquid form so can be directly used to top up the Flux Bath in between the galvanizing process.
- Increases the life of flux in flux bath.
- Easy and safe to use as no prior mixing is required and can be directly poured in the flux bath which saves time and labour
Specification of Leveling flux (Recharging flux) is as below
| Particulars | Observations |
| Colour and Appearance | Crystal Clear solution |
| Zinc Chloride solution to Ammonium Chloride Ratio | 3:1 |
| Additives (Approximately) | 5 % |
| Iron impurities | less than 3 ppm. i.e. 0.0003% on 100% Basis |
| Specific Gravity | 1.33 to 1.40 |
| Be | 35 to 42 |
| pH of solution | 4 to 4.5 |
| Consumption | Approximately 1 to 2 Kgs. Per ton of galvanized material |
| Packing | In HDEP Carbuoys or Tanker Load as required. |
| Usage | Ready to Use. No prior mixing is required. |